Stainless steel owes its corrosion resistance to a minimum of about 10.5% chromium, which forms a thin, self-healing oxide film on the surface. Additions of nickel, molybdenum, nitrogen, titanium and niobium tailor each grade for strength, weldability, pitting resistance or high-temperature service.
Rajdeep Metals supplies the full working range — from general-purpose 304/304L and chloride-resistant 316/316L, through stabilised 321 and 347 and heat-resistant 310S, to 904L and the high-strength duplex grades 2205 and 2507. We help you balance service conditions against cost before you order.
| Seamless & Welded Pipe | ASTM A312 / ASME SA312, A358, A790 (duplex), A928 (duplex welded) |
|---|---|
| Tubes | ASTM A213, A249, A269, A270 (sanitary), A789 (duplex) |
| Sheets, Plates & Coils | ASTM A240 / ASME SA240, A480 (general requirements) |
| Rods & Bars | ASTM A276, A479 / ASME SA479, A484 |
| Buttweld Fittings | ASTM A403 WP304/316/321/347, A815 (duplex) — ASME B16.9, B16.28, MSS SP-43 |
| Forged Fittings & Flanges | ASTM A182 F304/F316/F321/F347/F310/F51/F53 — ASME B16.11, B16.5, B16.47 |
| Fasteners | ASTM A193 B8 / B8M, A194 Gr. 8 / 8M, A320 B8 / B8M |
| Wire | ASTM A580, A313 (spring wire), AWS A5.9 (filler wire) |
| Dimension Standards | ASME B36.19M, B36.10M, EN 10216-5, EN 10217-7 |
| Grade | C | Mn | Si | P | S | Cr | Ni | Mo | Other |
|---|---|---|---|---|---|---|---|---|---|
| 304 | 0.08 | 2.00 | 0.75 | 0.045 | 0.030 | 18.0 – 20.0 | 8.0 – 10.5 | — | N 0.10 |
| 304L | 0.030 | 2.00 | 0.75 | 0.045 | 0.030 | 17.5 – 19.5 | 8.0 – 12.0 | — | N 0.10 |
| 316 | 0.08 | 2.00 | 0.75 | 0.045 | 0.030 | 16.0 – 18.0 | 10.0 – 14.0 | 2.00 – 3.00 | N 0.10 |
| 316L | 0.030 | 2.00 | 0.75 | 0.045 | 0.030 | 16.0 – 18.0 | 10.0 – 14.0 | 2.00 – 3.00 | N 0.10 |
| 321 | 0.08 | 2.00 | 0.75 | 0.045 | 0.030 | 17.0 – 19.0 | 9.0 – 12.0 | — | Ti 5×(C+N) – 0.70 |
| 347 | 0.08 | 2.00 | 0.75 | 0.045 | 0.030 | 17.0 – 19.0 | 9.0 – 13.0 | — | Nb 10×C – 1.00 |
| 310S | 0.08 | 2.00 | 1.50 | 0.045 | 0.030 | 24.0 – 26.0 | 19.0 – 22.0 | — | — |
| 904L | 0.020 | 2.00 | 1.00 | 0.045 | 0.035 | 19.0 – 23.0 | 23.0 – 28.0 | 4.0 – 5.0 | Cu 1.0 – 2.0 |
| 2205 (S32205) | 0.030 | 2.00 | 1.00 | 0.030 | 0.020 | 22.0 – 23.0 | 4.5 – 6.5 | 3.0 – 3.5 | N 0.14 – 0.20 |
| 2507 (S32750) | 0.030 | 1.20 | 0.80 | 0.035 | 0.020 | 24.0 – 26.0 | 6.0 – 8.0 | 3.0 – 5.0 | N 0.24 – 0.32, Cu 0.50 |
Limits for other product forms (A312 pipe, A276 bar, A182 forgings) differ slightly — the governing specification is always stated on the mill test certificate.
| Grade | Tensile Strength (MPa) | Yield Strength 0.2% (MPa) | Elongation in 50 mm (%) | Hardness (HB max) |
|---|---|---|---|---|
| 304 | 515 | 205 | 40 | 201 |
| 304L | 485 | 170 | 40 | 201 |
| 316 | 515 | 205 | 40 | 217 |
| 316L | 485 | 170 | 40 | 217 |
| 321 | 515 | 205 | 40 | 217 |
| 347 | 515 | 205 | 40 | 201 |
| 310S | 515 | 205 | 40 | 217 |
| 904L | 490 | 220 | 35 | — |
| 2205 (S32205) | 655 | 450 | 25 | 293 |
| 2507 (S32750) | 795 | 550 | 15 | 310 |
Duplex grades offer roughly twice the yield strength of 304/316, which often allows thinner walls for the same design pressure.
| Grade | UNS | Werkstoff Nr. | EN | JIS |
|---|---|---|---|---|
| 304 | S30400 | 1.4301 | X5CrNi18-10 | SUS 304 |
| 304L | S30403 | 1.4307 | X2CrNi18-9 | SUS 304L |
| 316 | S31600 | 1.4401 | X5CrNiMo17-12-2 | SUS 316 |
| 316L | S31603 | 1.4404 | X2CrNiMo17-12-2 | SUS 316L |
| 321 | S32100 | 1.4541 | X6CrNiTi18-10 | SUS 321 |
| 347 | S34700 | 1.4550 | X6CrNiNb18-10 | SUS 347 |
| 310S | S31008 | 1.4845 | X8CrNi25-21 | SUS 310S |
| 904L | N08904 | 1.4539 | X1NiCrMoCu25-20-5 | — |
| 2205 | S32205 | 1.4462 | X2CrNiMoN22-5-3 | SUS 329J3L |
| 2507 | S32750 | 1.4410 | X2CrNiMoN25-7-4 | — |
Equivalents are for reference; chemistry and property limits are not always identical between standards.
Tell us the medium, temperature and pressure — we will suggest the right grade and confirm stock.